Maybe I'm worrying too mutch.
The big gap if I screw up two Tokins together, is about 0.5 mm at the screwholes. If I measure gap perpendicular to the SITs longer side, it is decreases in a short way below 0.05 mm.
It is quite interesting at the same time, if I try to measure at the shorter side, I almost able to put through 0.05mm gap meter.
So this side is concave a littlebit.
I think, Soundhappy is right, when he recommend Kerafoil.
Mica too hard in this case, while Kerafoil 0.25 will be able to fill the gap.
Yet, it would be nice, if we know the recommended torque settings.
This is what I was trying to talk about:
Attachments
So, I revised my previous viewpoint. I will use mica and goop.
I will use sandpaper before to reach a smooth plane.
Anyway, Keratherm-Kerafoil quite pricey, on that money I will buy some lottery rather.
I will use sandpaper before to reach a smooth plane.
Anyway, Keratherm-Kerafoil quite pricey, on that money I will buy some lottery rather.
@ Gyuri
You have 4 thermal pads for big Tokins from this
Kerafol 86/82 Thermally conductive film 0.25 mm 6.5 W/mK (L x W) 100 mm x 100 mm | Conrad.com
Kerafol ( brand name ) Keratherm ( product name ) high quality, price is not extravagant
You have 4 thermal pads for big Tokins from this
Kerafol 86/82 Thermally conductive film 0.25 mm 6.5 W/mK (L x W) 100 mm x 100 mm | Conrad.com
Kerafol ( brand name ) Keratherm ( product name ) high quality, price is not extravagant

So, I revised my previous viewpoint. I will use mica and goop.
I will use sandpaper before to reach a smooth plane.
Anyway, Keratherm-Kerafoil quite pricey, on that money I will buy some lottery rather.
Mica and goop do the job as well 😀 Most important is get use of the large size heat sinks
The original from Michael Rothacher look a little bit like this too, except for all the guts exposed 😉
If you have not seen it here it is : Frankentracer Part One - YouTube
Just ordered a roughly matched pair. Excited to see what Papa is cooking up!
Which did you end up going with?
Which did you end up going with?
These ones:
Roughly matched pair (with rough data)THF-51S (2SK77,2SK182) TOKIN SIT NOS | eBay
Thanks Gyuri 🙂
I keep original anodized metal protection layer.
Make up imperfections with small thermal paste goop layer is easy,
thermal film thickness can compensate as well.
Naked copper does easily oxidize and become grey green after a longer period of time.
Oxidation I am worry about.
I keep original anodized metal protection layer.
Make up imperfections with small thermal paste goop layer is easy,
thermal film thickness can compensate as well.
Naked copper does easily oxidize and become grey green after a longer period of time.
Oxidation I am worry about.
Good point, Soundhappy!
And there is an eternal question:
If we would like to make a plain and smooth surface, how smooth is we need?
If it will be like a glass surface, there will no remain goop between device and heatsink.
About oxidation, you are correct, I doesn't gave a tought to this viewpoint.
I hope so, on the fixed device with mica and goop it will be not an issue.
And there is an eternal question:
If we would like to make a plain and smooth surface, how smooth is we need?
If it will be like a glass surface, there will no remain goop between device and heatsink.
About oxidation, you are correct, I doesn't gave a tought to this viewpoint.
I hope so, on the fixed device with mica and goop it will be not an issue.
- Home
- Amplifiers
- Pass Labs
- While they last...