On the mat it gets to a fine tuning of your system. I like PVC and PVC lead sandwich in my system right now. But all the rest seem to play a different sonic role. The good news is you have a large heavy platter, your 90 % home now.
Tom
 
The platter and platen arrived today. The pics don’t do it justice. Nine and a half years to get to this point. The Teres Bearing instruction sheet is dated March ‘09.

Now to locate some #11 lead shot. May have to compromise here. That stuff is very hard to source.
 
Seth

I think I used #8. Not sure if anyone did listening test with different shot. I also did it dry. I know redpoint played with oil mixed in. You should be able to get shot at gun places and sportsman warehouse etc... Have fun!!!

Tom
 
Yeah. I can get #9. Anything smaller is unobtainium. Of course, the smaller the sphere, the more you can pack into a given cylinder. The greatest density involves a mix of sphere sizes. Some Russian geometer made a formula for that but the brain cells that retained that info died a while back.
 
Weight wise small is better. The fun begins with the vibration control. Small, large, combo, how much surface contact etc.etc.etc... And the bottom line when you get to the end of the math, is how does it sound? You should be between 30-40 lbs loaded, that seems to be a sweet spot.

Enjoy the ride
Tom
 
You do have the copper top. How thick is the platter? The outside is most important. Not sure hole size, how many, and how deep. How much does weigh now?

You should be able to do the math for a close total weight. Subtract the removed aluminum weight then add the lead weight and your home.

Tom
 
Hey Seth are the holes already drilled? If they are you could put lead shot in plastic bag and fill hole. Then pull it out and weight it, then multiply. This would save you the time of figuring volume. Forgot how much Chris said the bearing/ ball pad can take.

Tom
 
517E64C0-CD8F-4280-AE56-B8CECE76F7E5.jpg

5DDE8245-A5D5-4226-B7D6-2C89EB1CD830.jpg

The holes are 2.00 inches x 2.25 inches deep
 
Interesting.

I have been struggling with finishing options - my approach uses a combination of POM (Delrin) and Aluminium. Delrin is relatively easy to clean using isopropyl, but the aluminium platter, even when anodized, can sometimes "stain".

It turns out that the bearing oil I've found most success with (in my approach) is slightly alkaline, and that dissolves the oxide layer causing the "staining". Apparently I have trouble wiping the oil from my fingers before handling the platter. 🙂

Lacquering would be an interesting approach, but won't that chip?
 