superalloy ( 78% nickel/2%cobalt) EI-66 with Furukawa ultimate wire.
superalloy ( 78% nickel/2%cobalt) EI-66 with Furukawa ultimate wire.
Please consider donating to help us continue to serve you.

Ads on/off / Custom Title / More PMs / More album space / Advanced printing & mass image saving
Reply
 
Thread Tools Search this Thread
Old 22nd January 2006, 03:34 PM   #1
tube-lover is offline tube-lover  Hong Kong
diyAudio Member
 
Join Date: Jul 2004
Location: Hong Kong
Default superalloy ( 78% nickel/2%cobalt) EI-66 with Furukawa ultimate wire.

hi,

spec is 5K:5K 25ma.

recently I collect some 80% supermalloy EI-66 lamination with 0.08mm thick from the remain stock of nippon steel crop. It contain two type of element ~78% nickel & 2% of cobalt.

I also order Furukawa "TEX-F" is coated with three insulation( ultra thin insulate layer) which prepare to call Daburu to OEM 5K:5K 25ma interstage transformers for tube amp.

This interstage will very good for use 6c45,417a,437a,3a/167m,5842, E180F ( triode connect) etc

5K:5K 25ma was working well of high gm tubes such as above were only a few examples. Tubes with internal plate resistances around 2,000 ohms or less will work well with this Interstage.

spec is 5K:5K 25ma.

size of the core was EI-66X40

Pls saw the spec of the new wire.

"TEX-F" is coated with three insulation layers which are of dedicated polyether sulfone (a super engineering plastic) and enhanced in high-frequency V-t performance.

Features

Temperature Index: F type (155C)*1 under IEC 60172
Ultra-Thin Three fold Insulation (100m)
Wide Size Choice of 0.2 to 1.0mm (diameter)
Fine High-Frequency V-t Performance

Due to the core only 38pcs.

It means only can produce 19 pair of this type IT.

I would like to try groups order for this IT.

Pls understand superalloy is very very expensive.

Hand over time will 1 month.

Furukawa wire was special order which was paralell 4 pcs of wire. in parallel form, Factory funish, not litz form to lower the loss of the HF & prevent skin effect.

Fubish look was hammer tone full enclose outlook.

Sample test in spec 26Hz~68Khz -1.5db.

Group price will USD 360 per pair.

19 pairs only because limited of the core only 38 pcs.

Postage include by EMS world wide.

Photos show the core.

thx

thomas
Attached Images
File Type: jpg p1010329.jpg (62.4 KB, 296 views)
  Reply With Quote
Old 22nd January 2006, 03:35 PM   #2
tube-lover is offline tube-lover  Hong Kong
diyAudio Member
 
Join Date: Jul 2004
Location: Hong Kong
Talking superalloy ( 78% nickel/2%cobalt) EI-66 with Furukawa ultimate wire.

Hi,


more photos of the close up of the laminations.


thx


thomas
Attached Images
File Type: jpg p1010330.jpg (56.3 KB, 268 views)
  Reply With Quote

Reply


superalloy ( 78% nickel/2%cobalt) EI-66 with Furukawa ultimate wire.Hide this!Advertise here!
Thread Tools Search this Thread
Search this Thread:

Advanced Search

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump

Similar Threads
Thread Thread Starter Forum Replies Last Post
source of nickel + silicon steel laminations beetel Tubes / Valves 2 28th November 2012 10:36 AM
Needed: transformer core materials cobalt nickel arieknarie Tubes / Valves 0 27th February 2009 01:21 PM
I Need Nickel Iron Laminations and Bobbins ! Nikolas Ojala Swap Meet 3 7th April 2008 03:57 PM
Nickel ribbon APi Planars & Exotics 21 21st June 2006 06:49 AM


New To Site? Need Help?

All times are GMT. The time now is 04:53 PM.


Search Engine Optimisation provided by DragonByte SEO (Pro) - vBulletin Mods & Addons Copyright © 2019 DragonByte Technologies Ltd.
Resources saved on this page: MySQL 15.00%
vBulletin Optimisation provided by vB Optimise (Pro) - vBulletin Mods & Addons Copyright © 2019 DragonByte Technologies Ltd.
Copyright ©1999-2019 diyAudio
Wiki